Janus Membrane
Patent application specification · Walkthrough

Unitary Janus and tri-zone cis-1,4-polyisoprene membranes

A single, seamless elastomeric sheet in which the rubber tree's own chain-end chemistry is driven to opposite faces and locked there — no adhesive lamination, no vulcanization accelerators. Methods of manufacture, and the device families the asymmetry makes possible.

L1 · α-phospholipid face L2 · elastomeric core L3 · ω-peptide face 16 claims 9 examples 6 figures
Fresh white latex collected in a cup on a tapped rubber tree.
Hevea brasiliensis field latex — the feedstock whose heterotelechelic chain ends the invention exploits.

One sheet, two chemistries, no seam

In native Hevea rubber each cis-1,4-polyisoprene chain is heterotelechelic: a phospholipid group at the α-terminus, a peptide or protein residue at the ω-terminus. The invention treats that asymmetry as a manufacturing resource. Coalesce the latex between opposing boundary conditions, and the two chain ends sort to opposite faces; crosslink without accelerators, and the sorting becomes permanent.

01 · dispersed latex particles carry both termini; orientation is random 02 · directional coalescence hydrophobic / lipophilic boundary hydrophilic / polar boundary opposing interfacial conditions sort α- and ω-termini vertically 03 · accelerator-free lock e-beam · γ · UV · peroxide one continuous phase; gradient is now covalently fixed
Figure 1 Directional coalescence of aqueous Hevea latex particles bearing α-phospholipid and ω-peptide/protein termini between opposing interfacial boundary conditions, and subsequent accelerator-free crosslinking into a unitary tri-zone (L1/L2/L3) Janus membrane.
<20µg/dm² extractable protein

ASTM D5712, after protease trimming and washing (Example 1).

66°contact-angle differential Δθ

108° on L1 against 42° on L3; the claim floor is 30°.

≤10 µmconformable array thickness

Bending stiffness scales with t³, so thinness is the whole game.

0accelerators, 0 tie-layers

No thiurams, dithiocarbamates, MBT/MBTS, guanidines or thioureas.


Abstract

A unitary elastomeric membrane is formed from aqueous natural rubber latex or modified cis-1,4-polyisoprene by directing heterotelechelic α-phospholipid terminal groups toward a first major surface (L1) and ω-peptide or protein terminal groups toward an opposing second major surface (L3) across an intermediate core zone (L2), without multi-layer adhesive lamination. Locking the gradient by accelerator-free crosslinking — e-beam, gamma or UV photo-crosslinking — yields a low-allergen, low-sensitizer membrane supporting orthogonal modifications: zwitterionic anti-fouling coatings, conformationally switchable protein and aptamer gates, asymmetric CNT / silica / PEDOT:PSS composites, micro-perforated one-way wound dressings, ≤10 µm neural and wearable electrodes, gas-permeable cyclic-stretch bioreactors, strain-gated drug delivery, and doxycycline-regulated reprogramming-factor delivery systems.

Field of the invention

Elastomeric polymer membranes and bio-interfacial materials; more particularly unitary, asymmetric (Janus and tri-zone) elastomeric membranes formed from natural rubber latex or synthetic polyisoprene via directional coalescence and network stabilization, methods of manufacturing such membranes across diverse processing regimes, and standalone or conjunctive devices using them.

Figures at a glance

FIG. 1 — Coalescence

Latex particles sorted between opposing boundaries, then locked. Overview tab.

FIG. 2 — Process routes

Film-forming modalities, micro-structuring and cure. Manufacture tab.

FIG. 3 — Functionalization

Orthogonal face chemistry and the switchable pore gate. Surfaces tab.

FIG. 4 — ECoG array

Traces on L3, windows through L1. Applications tab.

FIG. 5 — Stretch & release

Cyclic-stretch bioreactor and strain-gated patch. Applications tab.

FIG. 6 — Gated delivery

Pulsed small-molecule metering across the membrane. Applications tab.